    nope.....but they did use 531 to make the jaguar D-Type chassis and I read that 953 is used as a layer in bullet-proof jackets...also:
    Peter Thompson from Carpenter Specialty Alloys (Reynolds’ material supplier), 953 stainless alloy is twice as strong as titanium with a frame weight comparable to high-end aluminum, and won’t corrode.

    But if you are worried about dents, surely you specify a greater wall thickness no?