I was teaching cold forming in class and realised I could probably make an expedition-style bagman like this one, rather than buying it for £40+.....
What material/gauge are you using?
Used here is the original tubing, as I couldn't get it out of the mount.
I bought some 7mm ti rod to use. I'm gonna see if Caradice will sell me just the lower section of the clamp to make another one, but then again this may just work so I'm not 100% sure yet.