Midway through renovating a 60s bungalow and I need to prime and paint 7x doors and door frames, is there a forum approved knotting solution and primer? or does the use of a primer negate the need for knotting solution? Thanks for all the help and advice over the years from this section of the forum.
Gently heating the knots will tell you if they need treating if you are unsure.
Liberon do a knotting solution which for me at least turned some fucking awful sappy pine into something paintable that has since weathered well outdoors.
I wouldn't rely on primer alone tbh, even the spot-prime BIN.
Midway through renovating a 60s bungalow and I need to prime and paint 7x doors and door frames, is there a forum approved knotting solution and primer? or does the use of a primer negate the need for knotting solution? Thanks for all the help and advice over the years from this section of the forum.