You are reading a single comment by @BrickMan and its replies. Click here to read the full conversation.
  • +1 for mapei self level, used 600 kg of it in workshop and its mostly held up 5 years later. Some better prep on my part and doing it in more stages (some parts are 30mm or more in depth, when I think its mean't to be 6-10mm max with that compound?) would have resulted in a better finish.

    Was easy to paint though afterwards and cost was about right.

    Buy or make nail spike sandals and get a nail spike roller on a big long handle is the best advise I'd give, trying to push it around with blades and brushs is not gonna go that well. Prep + temperature are everything.