Yeah sounds good, er70 joins many things so I'm sure it'll be fine on the filler front, unless something is stainless or especially hard, which is unlikely.
I wouldn't preheat, that's more applicable for stuff that's thicker, where there is a risk of the bead cooling at a drastically different rate to the rest or the part