You are reading a single comment by @Breso and its replies. Click here to read the full conversation.
  • Depends how good of a finish you want to achieve!

    Sand it/get it blasted > etch primer > 2k primer > sand > base coat(s) > 2k lacquer > wet sand > more 2k lacquer > wet sand > flow coat 2k lacquer > flat and polish if you can be bothered. (Other painters will have differing process I’m sure).

    Cost of decent materials will be a lot to do a decent job though, as you’ll have to buy a lot more than you need to use for such a small project.

    Any 2k product is proper nasty shit, so proper respirator and extraction is highly recommended.

    I’m shit at giving advice im afraid though, as I highly doubt the way I do things is what would be considered the ‘correct’ way by a lot of other painters. I’m sure @privatepatterson would be happy to provide a some more in depth advice!

  • Thank you!!

    Cost of decent materials will be a lot to do a decent job though, as
    you’ll have to buy a lot more than you need to use for such a small
    project.

    That was my concern, I was just wondering if it was easy to find companies that supply primer and lacquer in small quantity, modelling size kinda tubs.